Copper vs Aluminum PCB Base, Worked Out in Numbers

Through the board, the dielectric sets most of the thermal resistance. Copper earns its weight in spreading, pulse loads and thermal cycling.

Published by ChengYue on . 4-minute read.

For heat going straight down through a metal-core board, swapping the aluminium base for copper cuts the stack resistance by about 6 % on a 2 W/m·K dielectric, because the dielectric holds most of the resistance. Copper pays when heat has to travel sideways, when the load arrives in pulses, or when large ceramic parts see wide thermal cycling, and only if 3.3 times the base weight is acceptable. Otherwise a higher dielectric grade on aluminium does more.

Why the base metal barely changes vertical heat flow

A 1.5 mm aluminium base adds about 15 % to the resistance of a 100 µm, 2 W/m·K dielectric, and a copper base about half that. Resistance per unit area is thickness divided by conductivity, so the layers compare directly (generic example):

Dielectric: 0.100 mm / 2 W/m·K = 0.50 °C·cm²/W
Aluminium base, 1.5 mm at 200 W/m·K = 0.075 °C·cm²/W
Copper base, 1.5 mm at 390 W/m·K = 0.038 °C·cm²/W

Aluminium to copper takes the stack from 0.575 to 0.538 °C·cm²/W, a 6 % gain. Raising the dielectric from 2 to 3 W/m·K on the same aluminium base takes it to 0.408 °C·cm²/W, a 29 % gain. The base share grows with the grade: on an 8 W/m·K dielectric the stack goes from 0.200 to 0.163 °C·cm²/W, an 18 % gain. The interface material to the heatsink adds its own resistance on top and dilutes the base metal's share again. What each dielectric grade does to temperature rise is worked through in the thermal conductivity article.

Copper and aluminium material constants

Copper conducts about twice as well as the aluminium alloys used for metal-core boards, weighs 3.3 times as much and expands about 28 % less per kelvin.

Approximate room-temperature textbook values; the exact alloy is on the laminate datasheet
PropertyAluminiumCopperCu ÷ Al
Thermal conductivity, W/m·K140–230 (≈ 200 used here)390≈ 2
Density, g/cm³2.708.933.3
CTE, ppm/K23–24170.72
Specific heat, J/g·K0.900.3850.43
Heat capacity per volume, J/cm³·K2.433.441.4

A 100 × 100 mm board with a 1.5 mm base:

Volume = 100 × 100 × 1.5 mm = 15 cm³
Aluminium: 15 cm³ × 2.70 g/cm³ = 40.5 g
Copper: 15 cm³ × 8.93 g/cm³ = 134 g

Per square metre of 1.5 mm base that is 4.05 kg against 13.4 kg.

Cases that justify a copper base

  • Heat must travel well over 10 mm sideways to reach the heatsink. Lateral resistance is R = L / (k · A). Carrying heat 20 mm along a 10 mm wide strip of 1.5 mm base, with the heatsink only at the far end, gives 6.7 K/W in aluminium and 3.4 K/W in copper; at 5 W that is a 33 K rise against 17 K. For spreading, 1.5 mm of copper behaves like 2.9 mm of aluminium.
  • The load comes in pulses of roughly 0.1 s to a few seconds. Copper stores 1.4 times as much heat per unit volume. A 10 J pulse absorbed in a 10 × 10 × 1.5 mm block under the part raises it about 27 K in aluminium and 19 K in copper (adiabatic estimate, an upper bound). Much shorter pulses stay mostly in the package, foil and dielectric; much longer loads reach steady state, where the heatsink decides.
  • Large ceramic bodies see wide thermal cycling. Alumina expands at about 7 ppm/K. Across a 10 mm part cycled from −40 to +125 °C (165 K), the free expansion mismatch is 26 µm on aluminium and 17 µm on copper, about 37 % less strain for the solder joints to absorb.
  • The circuit copper is 3 oz (105 µm) or heavier. A copper base matches the foil's 17 ppm/K, so the laminate behaves less like a bimetal strip and bows less after reflow.

Cases where aluminium is enough

  • The heatsink sits directly under the hot parts. An LED dissipating 4 W on a 4 × 4 mm pad (25 W/cm²) over the 100 µm, 2 W/m·K dielectric sees 12.5 K across the dielectric, 1.9 K across an aluminium base and 1.0 K across copper, one-dimensional. Copper saves under 1 K.
  • Mass counts. Luminaires, vehicle lamps and anything under vibration: 40.5 g against 134 g per 100 × 100 mm board, and the extra mass loads every screw and solder joint when the board shakes.
  • Boards are routed, V-scored or punched in volume. Copper is gummier, wears drills and cutters faster and is harder to punch cleanly at 1.5 mm. It also costs more per kilogram, and the board needs 3.3 times the mass.

A better dielectric on aluminium, or a copper base?

If a 2 W/m·K aluminium board runs too hot, try the next dielectric grade before changing the base. Aluminium-base laminate comes in grades from 1.0 to 8.0 W/m·K and copper-base laminate goes up to 8 W/m·K. With the 100 µm example, aluminium at 5 W/m·K reaches 0.275 °C·cm²/W and at 8 W/m·K 0.200 °C·cm²/W, both well below copper at 2 W/m·K (0.538 °C·cm²/W). Copper with an 8 W/m·K dielectric gives 0.163 °C·cm²/W, so it pulls ahead once the dielectric is already at its top grade, or when the spreading, pulse or CTE cases above apply. A thinner dielectric also lowers resistance but costs breakdown voltage; see dielectric thickness and breakdown voltage.

Stack of copper-faced metal-core laminate sheets seen from the edge
Copper-faced laminate sheets. The base metal under the dielectric is chosen separately from the dielectric grade.

Base, dielectric grade and copper weight are separate choices, explained layer by layer on the technology page. To test both bases on your own fixture, set them up in the laminate selector and request samples of each.

Next step

Pick the grade, base, copper weight and sheet size in the selector and send it as a sample request. Or put a question about this note to us directly.

Open the laminate selector

More from the blog