How to Read a Metal Clad Laminate Datasheet, Row by Row
Thermal conductivity, impedance, breakdown, peel, Tg, CTI and UL ratings: what each row measures and how to compare two suppliers fairly.
Two metal clad laminate datasheets can be compared only row by row, and only where the test method and the condition behind each row match. Thermal conductivity, the headline figure, is the row most often measured in different ways, so two sheets both printed "2.0 W/m·K" can run at different temperatures on the same board.
Construction rows
Dielectric thickness
Dielectric thickness is the insulating layer between copper foil and metal base, in µm, usually measured on a cross-section. Thermal impedance and breakdown voltage both scale with it, so a thermal or electrical figure quoted without the thickness it was measured at is half a number.
Metal base and copper foil
Base alloy and thickness in mm, copper in oz or µm (1 oz is 35 µm). Check whether the copper is nominal foil weight or measured thickness after pressing.
Thermal rows
Thermal conductivity
Thermal conductivity (k) is a property of the dielectric material alone, in W/m·K. It comes from a steady-state stack test to ASTM D5470, from laser flash diffusivity to ASTM E1461 using k = α · ρ · cp (diffusivity × density × specific heat), or from a transient plane-source test such as ISO 22007-2. The transient methods measure the bulk resin and leave out the interfaces to copper and aluminium, so they commonly read higher than D5470 on the same material. A laser-flash k and a D5470 k are not comparable. What each grade does on a real board is in aluminum PCB thermal conductivity.
Thermal impedance
Thermal impedance is the temperature rise per watt per unit area across the dielectric, in °C·cm²/W, measured to ASTM D5470. It folds thickness and interface resistance into one number, which makes it the better row for comparing two laminates:
100 µm at 2.0 W/m·K: R = t / k = 100×10⁻⁶ / 2.0 = 5.0×10⁻⁵ m²·K/W = 0.50 °C·cm²/W
75 µm at 1.5 W/m·K: R = 75×10⁻⁶ / 1.5 = 5.0×10⁻⁵ m²·K/W = 0.50 °C·cm²/W
The "1.5 W" layer is thinner and passes heat exactly as well. It will also break down at a lower voltage.
Electrical rows
Breakdown voltage
Breakdown voltage is the voltage at which the dielectric punctures, in kV, ramped to failure under the IPC-TM-650 2.5.6 family or ASTM D149. Check three things: AC or DC (DC figures are usually higher for the same layer), the dielectric thickness of the sample, and whether the row is really breakdown or a withstand (hi-pot) pass held for a set time at a lower voltage. A withstand pass is not a breakdown value. The thickness link is worked through in dielectric thickness and breakdown voltage.
Volume and surface resistivity
Resistivity is given in MΩ·cm and MΩ, measured to IPC-TM-650 2.5.17.1 or a similar method. Look for the conditioning: as received, after humidity, or hot. A figure after damp heat says more about field behaviour than one taken dry at room temperature.
Mechanical and thermal-stress rows
Peel strength
Peel strength is the force to pull the copper off the dielectric, in N/mm or lb/in, tested to IPC-TM-650 2.4.8. As received, after thermal stress and hot are three different rows, and heavier copper peels higher than 1 oz foil on the same resin. Compare the after-thermal-stress value at the copper weight you will buy.
Thermal stress (solder float)
Solder float is a pass/fail row: a sample floated on solder, commonly at 288 °C for a stated number of seconds, then checked for blistering or delamination (IPC-TM-650 2.4.13). Read the time and the number of cycles. A single 10 s float is a light test for a board that will go through lead-free reflow twice.
Tg
Tg is the glass transition temperature of the dielectric resin, in °C, and says nothing about the aluminium. It is measured by DSC, TMA or DMA (IPC-TM-650 2.4.25, 2.4.24 and 2.4.24.4), and DMA typically reads higher than DSC on the same resin, so Tg figures from different methods cannot be ranked directly.
Safety and rating rows
CTI
Comparative tracking index is the highest voltage at which the surface survives 50 drops of electrolyte without tracking, tested to IEC 60112, in V. It sets the material group used for creepage distances; how much layout that buys is covered in high CTI FR-4.
Flammability
Flammability is usually given as UL 94 V-0, from a vertical burn test. The rating holds at the thickness it was tested at, so check that the minimum rated thickness covers your construction.
MOT / RTI
Relative thermal index (UL 746B) is a long-term ageing temperature for the material; maximum operating temperature (UL 796) applies to a board construction. A row reading "working temperature 140 °C" with no UL basis is a supplier claim.
Four numbers to put side by side
- Thermal impedance in °C·cm²/W, both measured to ASTM D5470.
- Dielectric thickness in µm, the one the thermal and electrical rows were measured at.
- Breakdown voltage in kV, same AC or DC basis, at that thickness.
- Peel strength after thermal stress, at your copper weight.
If a datasheet lacks any of the four, ask for it before sampling; sample sheets by grade, base, copper and voltage grade are requested through the selector.
Next step
Pick the grade, base, copper weight and sheet size in the selector and send it as a sample request. Or put a question about this note to us directly.
Open the laminate selector